IT-170GT PCB Fabrication for Multilayer Boards

IT-170GT PCB banner with a green board and plated mounting holes

Illustration of a multilayer PCB with plated holes.

ITEQ IT-170GT is a halogen-free, high-Tg laminate and prepreg system for rigid multilayer PCBs. The current datasheet lists a 185°C glass transition temperature by DSC and a 150°C maximum operating temperature for laminate thickness of at least 0.63 mm. For a thick board with plated connector holes, the material is one part of the reliability decision. The drill geometry, inner-layer bond and copper barrel still have to survive the assembly and service conditions.

Read the thermal numbers as separate design inputs

Thermal qualification has three different questions: how the material expands as it heats, what rating applies to the specified construction, and how the fabricated and populated board behaves through its actual temperature history. Those questions require different evidence.

What the IT-170GT datasheet establishes
Datasheet item Reported result How to use it
Tg (DSC) 185°C Identifies the glass transition by the stated method. It is not the continuous use rating.
Maximum operating temperature 150°C at laminate thickness ≥0.63 mm Read the UL 746 entry with its thickness condition. Do not infer it from overall board thickness or extend it to a populated product.
50–260°C Z-axis expansion 2.2% at 58% resin content; 1.7% at 48% Compares expansion of the tested laminate constructions over the stated interval.
Td and delamination time Td 380°C at 5% mass loss; T260 and T288 each >60 min Distinct laboratory tests. These are not reflow limits or cycle counts.
Dk and Df at 10 GHz 3.9 and 0.0095 55% resin content, IPC-TM-650 2.5.5.13; a separate specimen basis from the expansion entries.

Source: ITEQ IT-170GT datasheet, Rev. 1.0-26. The CCL row identifies IT-170GT; the prepreg row lists IT-170GTB. Verify construction codes and the applicable safety recognition when releasing the purchase specification.

What does the difference in resin content change?

The 58% specimen shows 0.5 percentage points more through-thickness expansion than the 48% specimen over the published interval. A multilayer board can combine several core and prepreg constructions, with copper patterns that constrain movement. The difference signals that stack composition matters; it does not give the local strain in a plated hole. Specify individual dielectric builds, copper weights and required resin fill. Do not simply select a lower resin content to reduce expansion if it leaves too little resin to fill the etched relief.

Design the connector hole for both fabrication and fit

In a thick multilayer board, the resin and reinforcement expand through the thickness during heating while the bonded copper barrel is constrained. The resulting stress can accumulate through repeated excursions. A thin section of copper, a drill defect or a poor connection to an internal land can become the local weakness. The inspection must therefore represent the hole family most at risk, which may be a smaller plated hole on the same panel rather than the main connector hole.

Hypothetical connector review. A 2.40 mm board calls for a 0.30 mm finished plated hole. If the proposed production drill diameter is 0.38 mm, the nominal board-thickness-to-drill ratio is about 6.3:1. Dividing by the finished diameter gives 8.0:1, a different quantity. The drill value helps review plating access; the finished-hole tolerance governs pin fit and functional acceptance. The calculation does not establish an allowable ratio or prescribe the drill allowance.

Give the fabricator the connector manufacturer’s finished-hole tolerance and annular-ring requirements along with the plated-hole table. In a mechanical drilling review, check registration to buried lands, tool wear and hole-wall quality. Drilling can smear softened resin over inner-layer copper; desmear and conditioning must expose the lands before metallization without creating unacceptable damage. The cross-section should sample copper continuity and minimum thickness through the barrel, including the middle of deep holes, plus the connection to representative internal lands.

For a press-fit connector, coordinate the finished hole, plating and insertion specification with the actual compliant pin. For a soldered connector, the joint must wet and fill according to the assembly requirement; a thick plane connected to the barrel can draw heat away. A change between press-fit and soldered pins can therefore change the fabrication drawing, coupon selection and assembly tooling.

IT-170GT PCB illustration showing three board layouts with gold pads

Multilayer PCB illustration. Qualification should represent the actual plated-hole construction.

Diagnose opens that appear only after heat

When an open appears after thermal exposure, first localize the failing net and check when the resistance changes. A continuity test after cooldown can miss an intermittent open. If the application calls for thermal qualification, define a coupon with the relevant hole types, the conditioning and exposure sequence, and when resistance will be measured. Use the applicable IPC-TM-650 methods and purchasing criteria agreed for the build. Typical laminate data do not set board acceptance thresholds.

  • Crack through the barrel wall: section the suspect hole at useful orientations and check whether the break passes through plated copper. Review barrel thickness distribution, hole geometry and the thermal history.
  • Separation at an inner-layer connection: inspect the specific land-to-barrel interface and look for drilling, smear removal or metallization evidence. Continuous copper on an adjacent barrel wall does not clear the suspect junction.
  • Unsound solder joint or poor pin contact: test across the joint or contact separately from the bare-board net. Investigate joint wetting, solder fill or the connector insertion conditions before applying a laminate change as a corrective action.

Preserve the failed unit and compare it with an unstressed specimen when practical. A section through a healthy plane of the same hole can miss a localized crack. Resistance monitoring, physical sectioning and inspection of the assembly answer different parts of the diagnosis.

PCB FABRICATION & ASSEMBLY

Planning an IT-170GT PCB build?

Highleap can review the board construction and assembly requirements together.

Include finished hole tolerances, board thickness and the thermal exposures expected at assembly and in use.

Request a fabrication and assembly review

Define the first article around the actual heat exposures

Separate the assembly exposure from the service duty cycle. Specify proposed reflow and through-hole soldering steps, planned rework exposures where relevant, and the operating and cycling conditions imposed by the product. Profile areas with different thermal masses on the populated build. A soldered connector near a large plane can heat more slowly than nearby small SMT parts, so a process adjustment must be checked at both locations.

Highleap Electronics reviews these requirements as part of the combined PCB fabrication and assembly scope. Include the controlled stack-up, drill and finished-hole requirements, connector drawings, qualification coupon, BOM and exposure plan in the manufacturing inquiry. The first-article plan can then identify which holes to section, when to monitor resistance and which connector checks belong after assembly.

Sabrina

About the Author

Sabrina

PCB Engineering Specialist at Highleap Electronics

Sabrina has over 18 years of experience in the PCB industry, with a strong background in CAM engineering and PCB file review. She supports PCB projects from prototype to volume production, focusing on manufacturability and process reliability.

Her work helps engineering teams reduce production risk and achieve stable, high-quality PCB manufacturing results.

Sabrina on LinkedIn

Highleap PCB and PCBA solutions - request a quote

Recommended Posts

How to get a quote for PCBs

Let‘s run DFM/DFA analysis for you and get back to you with a report. You can upload your files securely through our website. We require the following information in order to give you a quote:

    • Gerber, ODB++, or .pcb, spec.
    • BOM list if you require assembly
    • Quantity
    • Turn time

In addition to PCB manufacturing, we offer a comprehensive range of electronic services, including PCB design, PCBA, and turnkey solutions. Whether you need help with prototyping, design verification, component sourcing, or mass production, we provide end-to-end support to ensure your project’s success.

For PCBA services, please provide your BOM (Bill of Materials) and any specific assembly instructions. We also offer DFM/DFA analysis to optimize your designs for manufacturability and assembly, ensuring a smooth production process.

    Tell Us About Your PCB Project

    No design files yet? No problem. Share what you know, and we'll follow up if more details are needed.



    Upload files (optional)

    PCB files, BOM, PDF/STEP, TXT, images, ZIP/RAR/7Z · Max 50 MB total